Molding

Greensand molds with gating system.

The black casting is iron and the others are aluminum.
Gating iron (Latin: ferrous) is different than gating aluminum or bronze (non-ferrous). Dross is produced with non-ferrous alloys , but NOT with iron. Dross is similar to the foam on top of beer.
When gating non-ferrous castings, dross is carried beyond the gate by the deep runner, clean metal enters the casting.
When gating iron, the metal is so heavy, 2 large openings (sprue/riser) are used to equalize the pressure.

Parameters of Gating
Alum castings 3lbs. or less- Bronze castings 9lbs or less
1/2″ sprue, 1″x 1″ runner up to 10″ long.

Alum castings 3-8 lbs.- Bronze 9-24 lbs.
3/4″ sprue, 1.5″x 1.5″ runner up to 14″ long.

Alum castings over 8 lbs. Bronze over 24 lbs.
1″ sprue, 2″x 2″ runner up to 18″ long.

Continue reading “Molding”

Gallery

Bronze is a mixture of copper and tin, brass is copper and zinc. Other elements are added in small quantities to give certain properties to alloys. There are over 400 copper based alloys used today. Some are for casting, others are for extruding.
Recyclers call it “red-brass”(bronze) or “yellow-brass”(brass).
see more

Patterns

A casting is a copy of your “pattern”. Sand is packed around the pattern and carefully removed. A slight draft is necessary on vertical surfaces (sides), like the way “stacking cups” work. Patterns can be made of wood, plastic or metal. Wood patterns should be sealed to prevent moisture being robbed from the sand. Shellac or paint work well.

When making a pattern, increase size 2% for shrink and a % for machining, depending on finish.

https://en.wikipedia.org/wiki/Pattern_(casting)