Molding tools

 1.Molding Flask, free plans here!

 2.Riddles            Sieve or screen

 3. Hole Formers (cutters)
 
1/8" wood dowel (vents), 1/4" wood dowel (pop-up), 1/2" copper pipe (sprue).......with items larger than 8" use a  3/4" copper pipe. All hole formers are sharpened on one end.          

4. Rammer/Straight edge (striker)  .75" x1.5" x14" wood       

 5. Runner bar pattern    .75" x.75" x 6" wood, sides are slightly angled at about 3 degrees, shellacked or painted.         

6. Molding Spoon Souvenir  or baby spoon   

7. Trowel

8. Parting Dust  In a sock or cloth bag.